What is the smelting process of 09CuPCrNi-A rusty steel

home > News

What is the smelting process of 09CuPCrNi-A rusty steel

The company regularly holds sales elites to share experiences, to promote the rapid growth of colleagues, and achieve the company and employees. The company conducts employee skill training and related knowledge video learning from time to time. All these things is to improve the employees' skills and literacy, and reflects its own value. It has always been the pursuit of BBN steel to enhance the employee’s ability and keep up with the times.

What is the difference between 20G and 20# steel grade? The difference between 20G and 20# steel is very big. The chemical elements, mechanical properties, service environment and price of 20G and 20# steel are very different. 09CuPCrNi-A rusty steel, 20G and 20# steel can not be compared. They are not of the same grade level, and can not be replaced by each other. 20# steel is high quality carbon structural steel, 20G steel is high pressure boiler steel. 09CuPCrNi-A rusty steel, 20# steel does not bear pressure, while the use temperature of 20G steel is 450~480℃.

Rolling of steel plates is the core of the entire steel rolling production process. The billet is deformed by rolling. The rolling process plays a decisive role in product quality. The quality requirements of rolled 09CuPCrNi-A rusty steel products include the three aspects of product geometry and dimensional accuracy, internal organization and performance, and product finish. Finishing: It is the last process in the 09CuPCrNi-A rusty steel rolling process, and it is also a more complicated process. It plays a final role in guaranteeing the quality of the product.

09CuPCrNi-A rusty steel, Grade P295GH chemical composition under EN10028-2:2003 is displayed as follows. Chemical composition (C: 0.08 to 0.20; Cr: ≤0.30; Si: ≤0.40; Cu: ≤0.30;Mn: 0.90 to 1.50; Mo: ≤0.08;P: ≤0.025; Nb: ≤0.020;S: ≤0.015; Ni: ≤0.30;Al: ≤0.020; Ti: 0.03; N: ≤0.012; Vi: ≤0.02). The yield Strength MPa (min) of P295GH steel plate with thickness less than 16mm is 295MPa, and the tensile strength is 460-580MPa.

Using advanced logistics management, advanced models and management experience to increase the reliability of logistics operations and provide customers with 24/7 cargo management. On the premise of reducing transportation and management costs as much as possible, we provide customers with high-quality and efficient services; good business reputation has been recognized and supported by our customers.

We are experienced shipbuilding and marine grade steel materials supplier and exporter with more than 20 years experience. For any question about the 09CuPCrNi-A rusty steel shipbuilding steel materials, such as shipbuilding steel price, ABS EH36 steel specification, Lloyds grade A steel properties, AH36 steel mechanical properties, AH32 steel price, DH32 steel dimensions, difference between EH36 and DH 36 etc., please feel free to consult us.

Ask for the instant quotation