The company adheres to the S355J0WP steel yield strength business tenet of "integrity casting strength, cooperation creating win-win", takes value-added service of supply chain as the tenet, and under the premise of existing market, bulk trade, logistics distribution and other advantages, develops a new comprehensive steel industry model combined with informatization. And will continue to provide customers with high-quality steel products and good service. We sincerely welcome new and old customers to join hands with our company S355J0WP steel yield strength and seek common development!

Low alloy coils are steel coils made of steel with a low alloy content, usually less than 3.5%. Low alloy coil materials mainly include A572 Gr 50, S355JR, SS490, ST52-3, Q345B, etc.. These grades are also the most widely used and produced low-alloy high-strength steel grades in the world. The strength of low alloy coils is about 20% to 30% higher than that of ordinary carbon structural steel, S355J0WP steel yield strength. And the atmospheric corrosion resistance of low alloy coils is 20% to 38% higher than that of ordinary carbon structural steel.

S355J0WP steel yield strength, High-strength wear-resistant plates have outstanding performance advantages. First of all, the high-strength wear-resistant plates get their name because their wear resistance is very good, and the degree of wear will not be prominent. Secondly, the corrosion resistance of the high-strength wear-resistant plate is very good. General chemical plants have many corrosive liquids, and the high-strength wear-resistant plates can be used as the floor to reduce risk of accidents.

The common delivery status of S355J0WP steel yield strength, SA516 Gr 70 plate is as follows:
1) SA516 Gr 70 plate quenching: the process of rapid cooling after heating to the temperature above the phase transformation point.
2) SA516 Gr 70 plate normalizing: after heating above the phase transition temperature, it is cooled normally (in air).
3) SA516 Gr 70 plate annealing: heating to above the phase transition temperature, cooling slowly.
4) SA516 Gr 70 plate tempering: after quenching, it is heated to a certain temperature (lower than the quenching temperature), kept warm, and then cooled.

S355J0WP steel yield strength, 15CrMo alloy steel is Chinese material. It is characterized by high Chrome and Molybdenum contents. The 15CrMo alloy steel chrome content is 0.80-1.10, and molybdenum content is 0.40-0.55. Besides, 15CrMo carbon content is 0.12-0.18, silicon content is 0.17-0.37, manganese content is 0.40-0.70. The heating temperatures for quenching and tempering of 15CrMo alloy steel are 900 and 650 centigrade respectively. The yield point of 15CrMo alloy steel is 295Mpa.

We are committed to providing customers with high-quality services, high-precision products and efficient solutions. If you have any demand for S355J0WP steel yield strength steel plate, steel pipe and other products, please contact us directly. We are willing to provide you with relevant product knowledge and specific specifications for free. Welcome to purchase.

The company's after-sales service team is a high-quality professional team. Most after-sales employees have rich service experience and have reached the level of after-sales engineer. The after-sales department implements the after-sales personnel responsibility system and a 24-hour response mechanism. The company's advanced customer relationship management system provides customers with "standardized and streamlined services". A sound customer relationship maintenance system, and a "one-stop" customer satisfaction tracking system, all reflect our strong after-sales service guarantee.

Ask for the instant quotation